Back half of model lifted off bed
rhaub101
Posts: 89🌟 Super Member 🌟
this started after about 2hrs into the print. Bed temp=67c
Comments
In my (close to two weeks of) experience the most influence on Bed adhesion has:
- Nozzle temp (<=205 C no adhesion, 210 C ok adhesion, 230 C crazy adhesion with my pla)
- closeness of nozzle to bed on 1st layer, the more your first layer gets squished on the bed the stronger it adheres
Warping is mostly caused by bed adhesion and cooling.
I set my FAN to max out at 3.5 to 4mm to get rid of warping.
I have never a problem with adhesion with PLA, but i do the following:
Bed temp first layer = 80 deg. all other = 60 deg.
All layers hight = 0.2 mm.
Flow first Layer = 110%, all other 90%
Nozzle temp first layer = 220 deg. all other = 190 deg.
First layer speed = 30 mm/s, all other = 70 mm/s.
Before printing, cleaning bed with alkohol.
Bed and fan are original JGaurora A5.
For less noise, I removed the "3d Printer" sheet.
I use Cura 3.6.0. is very goooooood!
Test it and have fun.
---- I forgot to say, i print all only with skirt, it works for the "Treefrog" very good.
You find it: https://www.thingiverse.com/search?q=Treefrog&dwh=865bf6d61901beb
Howdy, Stranger!
RegisterIt looks like you've been lurking for a while.
If you register, we will remember what you have read and notify you about new comments. You will also be able to participate in discussions.
So if you'd like to get involved, register for an account, it'll only take you a minute!